The injection moulding cycle, sprues, runners and gates, wall thickness, draft angles and ribs, a mould cost calculation, and extrusion and stretch blow moulding.

What you need to know

Answer each one before you reveal it.

Your recallNot started
Key term

Describe how the polymer is melted and injected in injection moulding.

Key term

What happens in injection moulding after the mould cavity has been filled?

Key term

Why is an injection mould water-cooled?

Questions from this subtopic

Each one with the model answer underneath.

  1. 1

    Describe how the polymer is melted and injected in injection moulding.

    Model answer

    Polymer granules are melted by heater bands and a rotating screw inside a barrel. The screw then rams the melt under high pressure into a closed, cooled mould.

  2. 2

    What happens in injection moulding after the mould cavity has been filled?

    Model answer

    Pressure is held while the part cools, packing in extra melt as the polymer shrinks. The mould then opens and ejector pins push the solid part out.

  3. 3

    Why is an injection mould water-cooled?

    Model answer

    Water channels in the mould remove heat so the part solidifies quickly. A shorter cooling time gives a shorter cycle and a higher output.

  4. 4

    What are the sprue, runners and gates in an injection mould?

    Model answer

    The sprue carries melt from the nozzle into the mould, and runners distribute it to each cavity. A gate is the narrow entry into each cavity.

  5. 5

    Why should an injection-moulded part have an even wall thickness?

    Model answer

    Thick sections cool and shrink more slowly than thin ones. Uneven walls cause sink marks, warping and longer cycle times.

  6. 6

    Explain why draft angles are designed into injection-moulded products.

    Model answer

    A draft angle is a slight taper on the faces that run in the direction the mould opens. The taper lets the part release from the mould without scraping or sticking.

Other ways to work this

The same content, four other ways.

Everything in your subscription

Runs, plus a mode for every other kind of session.

1Flash
2Imposter
3Fade
4Brain dump

Learn every subtopic in runs of four questions

Facts flash and fade, a wrong word hides in some of them, and a brain dump decides which questions are locked in.

Material Selection and Wood
Metals
Plastics
Composite and Emerging Materials

Cram the night before, weakest topic first

A quick scan finds your weakest topics. Recall each fact you missed three times in a row.

The output voltage is V.
356

Blank Blitz consolidates the facts

Rapid timed gap-fills on the terms and numbers you need to recall without thinking.

✓What it iscovered
~Why it happenspartly there
How long it lastsnot there yet

Explain It tests your understanding

Explain a concept in your own words and see which of its points you covered.

Hazard means anything with the potential to cause harm.
TrueFalse

Test It catches misconceptions

Spot the fault in a statement. The faults are the mistakes students make most often.

721941163128510

Brain Breaks between sessions

Short focus games to reset attention, so the next set lands better than the last.

Every question in Processing Materials, on a schedule.

Learn it in runs of four questions, each ending on a brain dump against the clock. Every question you lock in comes back the next day, then at longer gaps, each time just before you would forget it.

Or £46 a year, about £3.83 a month. Cancel anytime.